Polymer Property : Dielectric Strength = 18.5 kV/mm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 18.5 kV/mm

@Thickness 3.20 mm
470 kV/in

@Thickness 0.126 in
in air; ASTM D 149
SABIC Innovative Plastics Valox® 357 PBT
PC/PBT, Unreinforced, impact modified, UL94V-0 rated. Applications like bobbins, switches and enclosures.This data was supplied by SABIC-IP for the Americas region.
Dielectric Strength 18.5 kV/mm

@Thickness 3.20 mm
470 kV/in

@Thickness 0.126 in
in oil; ASTM D 149
SABIC Innovative Plastics Valox® 357 PBT
PC/PBT, Unreinforced, impact modified, UL94V-0 rated. Applications like bobbins, switches and enclosures.This data was supplied by SABIC-IP for the Americas region.
Dielectric Strength 18.5 kV/mm

@Thickness 3.20 mm
470 kV/in

@Thickness 0.126 in
in air; ASTM D149
SABIC Innovative Plastics Valox® 357 PBT (Asia Pacific)
PBT + PC, Unreinforced, impact modified, UL94V-0 rated. Applications like bobbins, switches and enclosures.
Dielectric Strength 18.5 kV/mm

@Thickness 3.20 mm
470 kV/in

@Thickness 0.126 in
in oil; ASTM D149
SABIC Innovative Plastics Valox® 357 PBT (Asia Pacific)
PBT + PC, Unreinforced, impact modified, UL94V-0 rated. Applications like bobbins, switches and enclosures.
Dielectric Strength 18.5 kV/mm

@Thickness 3.20 mm
470 kV/in

@Thickness 0.126 in
in air; ASTM D149
SABIC Innovative Plastics Valox® 357 PBT+PC
PC/PBT, Unreinforced, impact modified, UL94V-0 rated. Applications like bobbins, switches and enclosures.
Dielectric Strength 18.5 kV/mm

@Thickness 3.20 mm
470 kV/in

@Thickness 0.126 in
in oil; ASTM D149
SABIC Innovative Plastics Valox® 357 PBT+PC
PC/PBT, Unreinforced, impact modified, UL94V-0 rated. Applications like bobbins, switches and enclosures.
Dielectric Strength 18.5 kV/mm

@Thickness 3.20 mm
470 kV/in

@Thickness 0.126 in
in air; ASTM D 149
SABIC Innovative Plastics Valox® 357M PBT (Asia Pacific)
This data was supplied by SABIC-IP for the Asia Pacific region.
Dielectric Strength 18.5 kV/mm

@Thickness 3.20 mm
470 kV/in

@Thickness 0.126 in
in oil; ASTM D 149
SABIC Innovative Plastics Valox® 357M PBT (Asia Pacific)
This data was supplied by SABIC-IP for the Asia Pacific region.
Dielectric Strength 18.5 kV/mm

@Thickness 3.20 mm
470 kV/in

@Thickness 0.126 in
in air; ASTM D 149
SABIC Innovative Plastics Valox® 357U PBT
Unreinforced PBTP, UL94 V-0/5VA rated. Improved UV resistant version of VALOX 357. Nonblooming flame retardant.This data was supplied by SABIC-IP for the Americas region.
Dielectric Strength 18.5 kV/mm

@Thickness 3.20 mm
470 kV/in

@Thickness 0.126 in
in oil; ASTM D 149
SABIC Innovative Plastics Valox® 357U PBT
Unreinforced PBTP, UL94 V-0/5VA rated. Improved UV resistant version of VALOX 357. Nonblooming flame retardant.This data was supplied by SABIC-IP for the Americas region.
Dielectric Strength 18.5 kV/mm

@Thickness 3.20 mm
470 kV/in

@Thickness 0.126 in
in air; ASTM D149
SABIC Innovative Plastics Valox® 357U PBT (Asia Pacific)
Unreinforced PBTP, UL94 V-0/5VA rated. Improved UV resistant version of VALOX 357. Nonblooming flame retardant.
Dielectric Strength 18.5 kV/mm

@Thickness 3.20 mm
470 kV/in

@Thickness 0.126 in
in oil; ASTM D149
SABIC Innovative Plastics Valox® 357U PBT (Asia Pacific)
Unreinforced PBTP, UL94 V-0/5VA rated. Improved UV resistant version of VALOX 357. Nonblooming flame retardant.
Dielectric Strength 18.5 kV/mm

@Frequency 60.0 Hz
470 kV/in

@Frequency 60.0 Hz
short time, wet; ASTM D149
Sumitomo Bakelite North America E 8701A Short Glass Fiber Reinforced Epoxy
E 8701A is a fiberglass and mineral reinforced epoxy molding compound, with excellent dimensional stability and good strength at elevated temperatures.Information provided by Sumitomo Bak North Amer..
Dielectric Strength 18.5 kV/mm

@Thickness 3.20 mm
470 kV/in

@Thickness 0.126 in
in air; ASTM D149
SABIC Innovative Plastics Valox® 357U PBT+PC
Unreinforced PC/PBT, UL94 V-0/5VA rated. Improved UV resistant version of VALOX 357. Nonblooming flame retardant.
Dielectric Strength 18.5 kV/mm

@Thickness 3.20 mm
470 kV/in

@Thickness 0.126 in
in oil; ASTM D149
SABIC Innovative Plastics Valox® 357U PBT+PC
Unreinforced PC/PBT, UL94 V-0/5VA rated. Improved UV resistant version of VALOX 357. Nonblooming flame retardant.