Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 2.87 kV/mm @Thickness 3.17 mm |
73.0 kV/in @Thickness 0.125 in |
100% RH for 96 hours; ASTM D149 |
Garlock BLUE-GARD® 3300 Compressed Aramid Fiber Gasketing, Neoprene Binder Aramid fiber, high-temperature fillers, and neoprene (CR) binder. Handles service conditions with refrigerants and various petroleum-based oils. Excellent SealabilityUnique blend of aramid fibers, f.. |