Polymer Property : Dielectric Strength = 244 kV/in Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 9.61 kV/mm

@Temperature 121 °C,
Time 10800 sec
244 kV/in

@Temperature 250 °F,
Time 3.00 hour
0.125 in. thickness; ASTM D149
Garlock GYLON® 3545 Layered Microcellular PTFE Gasketing
Microcellular PTFE gasket with rigid PTFE coreHighly compressible PTFE outer layers seal under low bolt load- suitable for many non-metallic flangesCompressible layers conform to surface irregularit..