Electrical Properties Metric English Comments
Dielectric Strength 26.4 kV/mm

@Thickness 1.60 mm
671 kV/in

@Thickness 0.0630 in
in oil; ASTM D 149
SABIC Innovative Plastics Ultem 2200N PEI
20% Glass fiber filled Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Americas region.
Dielectric Strength 26.4 kV/mm

@Thickness 1.60 mm
671 kV/in

@Thickness 0.0630 in
in oil; ASTM D 149
SABIC Innovative Plastics Ultem 2200N PEI (Asia Pacific)
20% Glass fiber filled Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region.
Dielectric Strength 26.4 kV/mm

@Thickness 1.60 mm
671 kV/in

@Thickness 0.0630 in
in oil; ASTM D 149
SABIC Innovative Plastics Ultem 2200N PEI (Europe-Africa-Middle East)
20% Glass fiber filled Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Dielectric Strength 26.4 kV/mm

@Thickness 1.60 mm
671 kV/in

@Thickness 0.0630 in
in oil; ASTM D 149
SABIC Innovative Plastics Valox® 414 PBT (Asia Pacific)
40% GR, increased strength/stiffness vs unreinforced. Non-flame retardant. For appliance handles, spotlights, electric motors, pump housings etc.This data was supplied by SABIC-IP for the Asia Pacif..