Electrical Properties Metric English Comments
Dielectric Strength 29.6 kV/mm

@Thickness 1.00 mm
752 kV/in

@Thickness 0.0394 in
short time; IEC 60243-1
SABIC Innovative Plastics Lexan® 2814R PC (Europe-Africa-Middle East)
LEXAN 2814R is a high viscosity, 10% glass reinforced, flame retardant grade, especially developed to meet the CSTB M2 flammability rating.