Polymer Property : Dielectric Strength = 32.0 kV/mm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 32.0 kV/mm

@Thickness 0.800 mm
813 kV/in

@Thickness 0.0315 in
in oil; IEC 60243-1
SABIC Innovative Plastics Valox® ENH4560 PBT (Europe-Africa-Middle East)
Valox* ENH4560 resin is a non-brominated/non-chlorinated flame retardant product based on Valox* PBT resin.
Dielectric Strength 32.0 kV/mm

@Thickness 0.800 mm
813 kV/in

@Thickness 0.0315 in
in oil; ASTM D149
SABIC Innovative Plastics Valox® ENH4560 PBT (Europe-Africa-Middle East)
Valox* ENH4560 resin is a non-brominated/non-chlorinated flame retardant product based on Valox* PBT resin.
Dielectric Strength 32.0 kV/mm

@Thickness 0.800 mm
813 kV/in

@Thickness 0.0315 in
in oil; IEC 60243-1
SABIC Innovative Plastics Xenoy® XL1562 PBT+PC (Europe-Africa-Middle East)
XENOY XL1562 is an impact modified PBT+PC blend with outstanding chemical resistance, good UV stability and flow properties.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio..
Dielectric Strength 32.0 kV/mm

@Thickness 1.00 mm,
Temperature 23.0 °C
813 kV/in

@Thickness 0.0394 in,
Temperature 73.4 °F
IEC 60243-1
DuPont Performance Polymers Sorona® 3030G BK001 Polytrimethylene Terephthalate (PTT)  (Unverified Data**)&
Sorona® 3030G BK001 is a 30% glass reinforced black PTT resin containing 25% renewably sourced ingredients by weight (37% polymer basis) with good strength, stiffness and low warpage and superior s..
Dielectric Strength 32.0 kV/mm

@Thickness 1.00 mm,
Temperature 23.0 °C
813 kV/in

@Thickness 0.0394 in,
Temperature 73.4 °F
IEC 60243-1
DuPont Performance Polymers Sorona® 3030GV BK001 Polytrimethylene Terephthalate (PTT)  (Unverified Data**)
Sorona® 3030GV BK001 is a 30% glass reinforced black PTT resin containing 25% renewably sourced ingredients by weight (37% based on polymer only) with low warpage and superior strength, stiffness a..
Dielectric Strength 32.0 kV/mm

@Thickness 1.00 mm,
Temperature 23.0 °C
813 kV/in

@Thickness 0.0394 in,
Temperature 73.4 °F
IEC 60243-1
DuPont Performance Polymers Sorona® MT3401 NC010 Polytrimethylene Terephthalate (PTT)  (Unverified Data**)
Sorona® MT3401 NC010 is a medium toughened polytrimethylene terephthalate resin containing 29% renewably sourced ingredients by weight. It was initially coded SE38001.Information provided by DuPont..
Dielectric Strength 32.0 kV/mm

@Thickness 1.00 mm,
Temperature 90.0 °C
813 kV/in

@Thickness 0.0394 in,
Temperature 194 °F
IEC 60243-1
DuPont Performance Polymers Sorona® MT3401 NC010 Polytrimethylene Terephthalate (PTT)  (Unverified Data**)
Sorona® MT3401 NC010 is a medium toughened polytrimethylene terephthalate resin containing 29% renewably sourced ingredients by weight. It was initially coded SE38001.Information provided by DuPont..