Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 13.2 kV/mm @Frequency 60.0 Hz |
335 kV/in @Frequency 60.0 Hz |
step-by-step, wet; ASTM D149 |
Sumitomo Bakelite North America E 2748-9641D Short Glass Fiber Reinforced Epoxy E 2748-9641D is a mineral and short fiberglass filled epoxy molding compound.Information provided by Sumitomo Bak North America, Inc. |
|||
Dielectric Strength | 13.2 kV/mm @Frequency 60.0 Hz |
335 kV/in @Frequency 60.0 Hz |
step-by-step, wet; ASTM D149 |
Sumitomo Bakelite North America Epiall® 2061B-1 Mineral and Glass Filled Electrical Encapsulation Grade Epoxy Epiall 2061B-1 is a fiberglass and mineral reinforced epoxy molding compound, with excellent dimensional stability, good electrical insulation properties, and good strength.Information provided by S.. |