Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 1.40 kV/mm @Thickness >=3.00 mm |
35.6 kV/in @Thickness >=0.118 in |
24hr/23°C/50% RH+1hr/oil 90°C; Parallel; IEC 60245-1; IEC/EN 60893-2 6.1.3.2 |
Elektro-Isola Etronit IR Phenolic, Paper Reinforcement, Dark Brown, Sheets Description: High-voltage insulation material at mains frequency. High breakdown voltage in oil and reasonable breakdown voltage in air at normal air humidity. Very low water absorption.Application:.. |
|||
Dielectric Strength | 1.40 kV/mm @Thickness >=3.00 mm |
35.6 kV/in @Thickness >=0.118 in |
24hr/23°C/50% RH+1hr/oil 90°C; Parallel; IEC 60245-1; IEC/EN 60893-2 6.1.3.2 |
Elektro-Isola Etronit IV Phenolic, Paper Reinforcement, Yellow, Sheets Description: Grade for mechanical electrotechnical and high frequency purposes. Tropical grade, well suited for areas where high air humidity can be expected. Suitable as high-frequency insulation o.. |