Electrical Properties Metric English Comments
Dielectric Strength 39.0 kV/mm

@Thickness 0.800 mm
991 kV/in

@Thickness 0.0315 in
in oil; IEC 60243-1
SABIC Innovative Plastics Cycoloy® XCY620HS PC+ABS
PC+ ABS General Purpose Non-FR
Dielectric Strength 39.0 kV/mm

@Thickness 0.800 mm
991 kV/in

@Thickness 0.0315 in
in oil; IEC 60243-1
SABIC Innovative Plastics Cycoloy® XCY620S PC+ABS
PC+ ABS Automotive applications
Dielectric Strength 39.0 kV/mm

@Thickness 0.800 mm
991 kV/in

@Thickness 0.0315 in
in oil; IEC 60243-1
SABIC Innovative Plastics Cycoloy® XCY620S PC+ABS (Asia Pacific)
PC+ ABS Automotive applications
Dielectric Strength 39.0 kV/mm

@Thickness 0.800 mm
991 kV/in

@Thickness 0.0315 in
in oil; IEC 60243-1
SABIC Innovative Plastics Cycoloy® XCY620S PC+ABS (Europe-Africa-Middle East)
PC+ ABS automotive applications, excellent flow/impact balance, high heat resistance temperature and excellent properties retention after hydrolytic and heat aging.
Dielectric Strength 39.0 kV/mm

@Thickness 0.800 mm
991 kV/in

@Thickness 0.0315 in
in oil; IEC 60243-1
SABIC Innovative Plastics Valox® 310SE0 PBT (Europe-Africa-Middle East)
VALOX 310SE0 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings.
Dielectric Strength 39.0 kV/mm

@Thickness 1.60 mm
991 kV/in

@Thickness 0.0630 in
in oil; IEC 60243-1
SABIC Innovative Plastics Valox® V3500EX PBT (Europe-Africa-Middle East)
Unfilled PBT,Flame Retardant, good flow, high elongation at break for Extrusion applications (Monofilaments, Insulation Cables),Electrical Parts and Connectors
Dielectric Strength 39.0 kV/mm

@Thickness 1.60 mm
991 kV/in

@Thickness 0.0630 in
in oil; ASTM D149
SABIC Innovative Plastics Valox® V3500EX PBT (Europe-Africa-Middle East)
Unfilled PBT,Flame Retardant, good flow, high elongation at break for Extrusion applications (Monofilaments, Insulation Cables),Electrical Parts and Connectors
Dielectric Strength 39.0 kV/mm

@Thickness 1.00 mm,
Temperature 23.0 °C
991 kV/in

@Thickness 0.0394 in,
Temperature 73.4 °F
50%RH; IEC 60243-1
DuPont Performance Polymers Zytel® ST801 NC010A Nylon 66  (Unverified Data**)