Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 43.0 kV/mm @Thickness 1.00 mm |
1090 kV/in @Thickness 0.0394 in |
d.a.m.; IEC 60243-1 |
Lanxess Durethan® BKV 215 000000 Nylon 6-Copolymer, Glass Fiber Reinforced, Impact Modified PA 6-Copolymer, 15% glass fibers, injection molding impact modifiedInformation provided by LANXESS. |
|||
Dielectric Strength | 43.0 kV/mm @Thickness 1.00 mm |
1090 kV/in @Thickness 0.0394 in |
cond.; IEC 60243-1 |
Lanxess Durethan® BKV 215 000000 Nylon 6-Copolymer, Glass Fiber Reinforced, Impact Modified PA 6-Copolymer, 15% glass fibers, injection molding impact modifiedInformation provided by LANXESS. |