Polymer Property : Dielectric Strength = 4320 kV/in Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 170 kV/mm

@Thickness 0.0500 mm
4320 kV/in

@Thickness 0.00197 in
Amorphous Film; ASTM D149
Solvay Specialty Polymers AvaSpire® AV-722 Polyaryletherketone (PAEK)  (Unverified Data**)
AvaSpire AV-722 is an unreinforced polyaryletherketone (PAEK) that offers improved economics relative to PEEK while retaining most of PEEK's key performance attributes. AV-722 resin has been formula..