Polymer Property : Dielectric Strength = 5.59 kV/mm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 5.59 kV/mm

@Thickness 3.17 mm
142 kV/in

@Thickness 0.125 in
100% RH for 96 hours; ASTM D149
Garlock BLUE-GARD® 3000 Compressed Aramid Fiber Gasketing, Nitrile Binder
Aramid fiber, high-temperature fillers, and nitrile (NBR) binder.Excellent SealabilityUnique blend of aramid fibers, fillers, and a NBR rubber binder provides improved torque retention and lowered e..