Polymer Property : Dielectric Strength = 53.0 kV/mm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 53.0 kV/mm

@Thickness 0.500 mm
1350 kV/in

@Thickness 0.0197 in
Transformer Oil; IEC 60243-1
SYNTHOS Forsan® 449 Acrylonitrile Butadiene Styrene (ABS)
High flow, high gloss, suitable for electroplating.Applications: General purpose, intricate and thin-walled productsHousehold appliances, vacuum cleaners, heels, toys, fan grilles, etc.Synthos was f..
Dielectric Strength 53.0 kV/mm

@Thickness 0.500 mm
1350 kV/in

@Thickness 0.0197 in
Transformer Oil; IEC 60243-1
SYNTHOS Forsan® 573 L Acrylonitrile Butadiene Styrene (ABS)
Increased heat resistant, glossy, UV stabilized.Applications: Electrotechnics, automotiveHousehold appliances, office equipment, car interior parts, profiles, ABS sheets, etc.Synthos was formerly kn..