Polymer Property : Dielectric Strength = 556 kV/in Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 21.9 kV/mm

@Thickness 1.60 mm,
Temperature 23.0 °C
556 kV/in

@Thickness 0.0630 in,
Temperature 73.4 °F
500 V/s in oil; ASTM D149
Lavergne VYPET VNT 340 PET 40% Glass - Mineral Reinforced
Vypet VNT 340 is a 40% glass/mineral reinforced PET injection molding compound designed for electrical and structural applications, with High Dielectric StrengthFeatures: High temperature performanc..
Dielectric Strength 21.9 kV/mm

@Thickness 3.20 mm
556 kV/in

@Thickness 0.126 in
in air; ASTM D 149
SABIC Innovative Plastics Valox® 414 PBT (Asia Pacific)
40% GR, increased strength/stiffness vs unreinforced. Non-flame retardant. For appliance handles, spotlights, electric motors, pump housings etc.This data was supplied by SABIC-IP for the Asia Pacif..