Polymer Property : Dielectric Strength = 625 kV/in Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 24.6 kV/mm

@Thickness 1.57 mm
625 kV/in

@Thickness 0.0620 in
Cond A; ASTM D229 S.T.
Industrial Laminates/Norplex NP320E Cotton Fabric
Description: Similar to NP320 with improved moisture resistance. Suitable for electrical applications in moderate humidity conditions.Thickness Tested: 0.062", 0.125", and 0.500”
Dielectric Strength 24.6 kV/mm

@Thickness 1.57 mm
625 kV/in

@Thickness 0.0620 in
Cond A; ASTM D229 S.T.
Industrial Laminates/Norplex NP320U Cotton Fabric
Description: Utility version of NP320E. Meets most, but not all, NEMA properties for L and LE, and is not certifiable as a NEMA Grade.Thickness Tested: 0.062", 0.125", and 0.500"