Polymer Property : Dielectric Strength = 8.74 kV/mm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 8.74 kV/mm

@Thickness 1.59 mm
222 kV/in

@Thickness 0.0625 in
100% RH for 96 hours; ASTM D149
Garlock GYLON® 3545 Layered Microcellular PTFE Gasketing
Microcellular PTFE gasket with rigid PTFE coreHighly compressible PTFE outer layers seal under low bolt load- suitable for many non-metallic flangesCompressible layers conform to surface irregularit..