Electrical Properties Metric English Comments
Dielectric Strength 32.3 kV/mm

@Thickness 1.59 mm
820 kV/in

@Thickness 0.0625 in
in air; ASTM D149
Polymer Resources PEI-GP1 Polyetherimide, Flame Retardant
Polyetherimide, Flame Retardant, High Heat ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information..