Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Dielectric Strength = 914 kV/in Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 36.0 kV/mm

@Thickness 0.800 mm
914 kV/in

@Thickness 0.0315 in
in oil; IEC 60243-1
SABIC Innovative Plastics Cycoloy® CX1440 PC+ABS
CYCOLOY CX1440 is a general purpose PC+ABS blend specially developped for thin wall applications requiring weld line strength and high flow with a good balance of properties
Dielectric Strength 36.0 kV/mm

@Thickness 0.800 mm
914 kV/in

@Thickness 0.0315 in
in oil; IEC 60243-1
SABIC Innovative Plastics Cycoloy® CX1440 PC+ABS (Europe-Africa-Middle East)
CYCOLOY CX1440 is a general purpose PC+ABS blend specially developped for thin wall applications requiring weld line strength and high flow with a good balance of propertiesThis data was supplied by..
Dielectric Strength 36.0 kV/mm

@Thickness 1.00 mm,
Temperature 23.0 °C
914 kV/in

@Thickness 0.0394 in,
Temperature 73.4 °F
IEC 60243-1
DuPont Performance Polymers Sorona® 3015GV NC010 Polytrimethylene Terephthalate (PTT)  (Unverified Data**)
Sorona® 3015GV NC010 is a 15% glass reinforced PTT resin containing 31% renewably sourced ingredients by weight (37% based on polymer only) with low warpage and superior strength, stiffness and sur..
Dielectric Strength 36.0 kV/mm

@Thickness 1.00 mm,
Temperature 90.0 °C
914 kV/in

@Thickness 0.0394 in,
Temperature 194 °F
IEC 60243-1
DuPont Performance Polymers Sorona® 3015GV NC010 Polytrimethylene Terephthalate (PTT)  (Unverified Data**)
Sorona® 3015GV NC010 is a 15% glass reinforced PTT resin containing 31% renewably sourced ingredients by weight (37% based on polymer only) with low warpage and superior strength, stiffness and sur..
Dielectric Strength 36.0 kV/mm

@Thickness 0.800 mm
914 kV/in

@Thickness 0.0315 in
in oil; IEC 60243-1
SABIC Innovative Plastics Cycoloy® CX1440 PC+ABS (Asia Pacific)
CYCOLOY CX1440 is a general purpose PC+ABS blend specially developped for thin wall applications requiring weld line strength and high flow with a good balance of properties
Dielectric Strength 36.0 kV/mm

@Thickness 1.00 mm,
Temperature 23.0 °C
914 kV/in

@Thickness 0.0394 in,
Temperature 73.4 °F
IEC 60243-1
DuPont Performance Polymers Sorona® 3015G BK001 Polytrimethylene Terephthalate (PTT)  (Unverified Data**)&
Sorona® 3015G BK001 is a 15% glass reinforced black PTT resin containing 31% renewably sourced ingredients by weight (37% polymer basis) with good strength, stiffness and low warpage and superior s..