Electrical Properties | Metric | English | Comments |
---|---|---|---|
Insulation Resistance | 10000 - 1.00e+7 ohm | 10000 - 1.00e+7 ohm | |
Lehmann & Voss LUVOCOM® 3-7901 Polyamide 6, with glass fiber and carbon fiber Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Strong, stiff parts.dynamic stressElectrically conductive, suitable for continuous discharging of staticall.. |