Electrical Properties Metric English Comments
Insulation Resistance 1.20e+14 ohm
1.20e+14 ohm
Wet; after 16 hours at 130°C
Malvern Minerals Diallylphthalate with Vinyl Silane Treated Novakup® 1250 Quartz Filler
Product data demonstrates the effect of the Novakup® (lamellar quartz surface treated with 1.0% Z-6075 vinyl silane) filler. Separate entries demonstrate the effect of untreated Novacite® fil..