Electrical Properties | Metric | English | Comments |
---|---|---|---|
Insulation Resistance | 1.37e+13 ohm | 1.37e+13 ohm | Bellcore, Control - final reading; IPC B25A |
Indium Corp. 1075-EX VOC-Free Wave Solder Flux 1075-EX VOC-free, is a resin/rosin-free flux specifically developed for wave soldering, surface mount, mixed technology and through-hole electronic assemblies.1075-EX VOC-Free is a water-based, non-.. |