Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Insulation Resistance 1.40e+13 ohm
1.40e+13 ohm
Control - final; IPC B25A, Telcordia GR-78
Indium Corp. WF-7742 VOC-Free Wave Solder Flux
WF-7742 is a VOC-free, no-clean flux specifically developed for Pb-free wave soldering of surface-mount, mixed technology and through-hole electronics assemblies.WF-7742 is a water-based, non-flamma..