Electrical Properties | Metric | English | Comments |
---|---|---|---|
Insulation Resistance | 1.56e+13 ohm @Time 605000 sec |
1.56e+13 ohm @Time 168 hour |
IPC B24 |
Indium Corp. WF-7742 VOC-Free Wave Solder Flux WF-7742 is a VOC-free, no-clean flux specifically developed for Pb-free wave soldering of surface-mount, mixed technology and through-hole electronics assemblies.WF-7742 is a water-based, non-flamma.. |