Electrical Properties | Metric | English | Comments |
---|---|---|---|
Insulation Resistance | 1.81e+10 ohm @Time 86400 sec |
1.81e+10 ohm @Time 24.0 hour |
Control; IPC B25A |
Indium Corp. 3590-T Wave Solder Flux, No-Residue 3590-T is a low-solids, non-halide rosin/resin free flux designed to eliminate post-cleaning operations. The effective flux activators provide superior solderability of surface mount, mixed technol.. |