Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Insulation Resistance = 3.20e+12 ohm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Insulation Resistance 3.20e+12 - 4.50e+14 ohm
3.20e+12 - 4.50e+14 ohm
Average value: 1.30e+14 ohm Grade Count:17
Overview of materials for Thermoset Polyurethane, Adhesive
This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Adhesive". Each property range of values reported is minimum and maximum values ..
Insulation Resistance 3.20e+12 ohm
3.20e+12 ohm
Cured property; MIL-I-46058C
Aptek 2503-A/B Low modulus urethane conformal coating
APTEK 2503-A/B is an unfilled, two component, electrically insulating, transparent, flexible urethane coating system designed for the encapsulation and protection of electronic services mounted on p..