Electrical Properties | Metric | English | Comments |
---|---|---|---|
Insulation Resistance | 5.87e+9 ohm @Time 605000 sec |
5.87e+9 ohm @Time 168 hour |
Control; IPC B24 |
Indium Corp. 1075-EXR 44 Wave Solder Flux Wave Solder Flux 1075-EXR 44 is specifically developed for Pb-Free and Sn-Pb wave soldering of surface-mount, mixed-technology and through-hole electronic assemblies.1075-EXR 44 is a water-based, no.. |