Electrical Properties Metric English Comments
Insulation Resistance 6.20e+11 ohm

@Temperature 120 °C
6.20e+11 ohm

@Temperature 248 °F
50% RH
Cytec Cyply® 1002 Epoxy Fiberglass Composite, Isotropic
CYPLY® 1002 is a cured epoxy composite material based on a unique non-woven parallel filament construction. This type of construction minimizes filament stress abrasion that can shorten fatigue li..
Insulation Resistance 6.20e+11 ohm

@Temperature 120 °C
6.20e+11 ohm

@Temperature 248 °F
50% RH
Cytec Cyply® 1002 Epoxy Fiberglass Composite, Unidirectional
CYPLY® 1002 is a cured epoxy composite material based on a unique non-woven parallel filament construction. This type of construction minimizes filament stress abrasion that can shorten fatigue li..
Insulation Resistance 6.20e+11 ohm

@Temperature 120 °C
6.20e+11 ohm

@Temperature 248 °F
50% RH
Cytec Cyply® 1002 Epoxy Fiberglass Composite, Crossply
CYPLY® 1002 is a cured epoxy composite material based on a unique non-woven parallel filament construction. This type of construction minimizes filament stress abrasion that can shorten fatigue li..