Polymer Property : Insulation Resistance = 7.06e+13 ohm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Insulation Resistance 7.06e+13 ohm
7.06e+13 ohm
Control - initial; Standard Bellcore
Indium Corp. 3590-T Wave Solder Flux, No-Residue
3590-T is a low-solids, non-halide rosin/resin free flux designed to eliminate post-cleaning operations. The effective flux activators provide superior solderability of surface mount, mixed technol..
Insulation Resistance 7.06e+13 ohm
7.06e+13 ohm
Control - initial; Standard Bellcore
Indium Corp. 3590-TX Wave Solder Flux, No-Residue
Wave Solder Flux 3590-TX is a low-solids, non-halide rosin/resin free flux designed to eliminate post-cleaning operations. Very effective flux activators provide superior solderability, reduced def..