Electrical Properties | Metric | English | Comments |
---|---|---|---|
Insulation Resistance | >= 7.50e+7 ohm @Diameter 8.00 - 10.0 mm |
>= 7.50e+7 ohm @Diameter 0.315 - 0.394 in |
After immersion in water; IEC 1212-2 5.2 |
Hippe EP CC 31 Woven Cotton Cloth Reinforced Epoxy Resin - Round, Molded Tube and Rod Used in mechanical, electrical and electronic applications.Information provided by Hippe. |
|||
Insulation Resistance | >= 7.50e+7 ohm @Diameter 8.00 - 10.0 mm |
>= 7.50e+7 ohm @Diameter 0.315 - 0.394 in |
After immersion in water; IEC 1212-2 5.2 |
Hippe PF CP 32 Cellulose Paper Reinforced Phenolic Resin - Round, Molded Tube and Rod Used in electrical and mechanical applications. Good stability of electrical properties when exposed to normal relative humidity. Improved mechanical and electrical properties when compared to PF .. |
|||
Insulation Resistance | >= 7.50e+7 ohm @Diameter 8.00 - 10.0 mm |
>= 7.50e+7 ohm @Diameter 0.315 - 0.394 in |
After immersion in water; IEC 1212-2 5.2 |
Hippe PF CP 41 Cellulose Paper Reinforced Phenolic Resin - Round, Molded Tube and Rod Used in mechanical and electrical applications. Good stability of electrical properties when exposed to high relative humidity.Information provided by Hippe. |