Electrical Properties | Metric | English | Comments |
---|---|---|---|
Insulation Resistance | 8.00e+14 ohm | 8.00e+14 ohm | Insulation Resistance; MIL-I-46058C |
Humiseal 1B31 Acrylic Conformal Coating Humiseal 1B31 Acrylic Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesSelective chemical resistanceExcellent repairabilityMIL-I-46058C ApprovedPasses thermal shock test (MI.. |
|||
Insulation Resistance | 8.00e+14 ohm | 8.00e+14 ohm | Insulation Resistance; MIL-I-46058C |
Humiseal 1B31LSE Acrylic Conformal Coating Humiseal 1B31LSE Acrylic Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesSelective chemical resistanceExcellent repairabilityMIL-I-46058C Approval PendingPasses thermal sho.. |