Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Breakdown >= 4200 V
>= 4200 V
Withstand Voltage AC V
Fujipoly Industries FLAT-5TV-10-.75 silicone rubber fusible tape
Information provided by Fujipoly Industries
Dielectric Breakdown >= 4200 V
>= 4200 V
Withstand Voltage AC V
Fujipoly Industries FLAT-5TV-10-1.0 silicone rubber fusible tape
Information provided by Fujipoly Industries