Polymer Property : Magnetic Coercive Force, Hc = 2900 Oe
Polymer Property :
Magnetic Coercive Force, Hc =
2900 Oe
Product List
Electrical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties
Metric
English
Comments
Magnetic Coercive Force, Hc
2900
Oe
2900
Oe
Intrinsic
Alliance BIF-11 Bonded (Composite) Magnetic Material