Polymer Property : Magnetic Coercive Force, Hc = 3200 Oe Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Magnetic Coercive Force, Hc 3200 Oe
3200 Oe
Alliance C-8H Strontium Ferrite Ceramic Magnetic Material
Magnetic Coercive Force, Hc 3200 Oe
3200 Oe
Alliance C-9 Strontium Ferrite Ceramic Magnetic Material