Electrical Properties | Metric | English | Comments |
---|---|---|---|
Magnetic Coercive Force, Hc | 3500 Oe | 3500 Oe | Intrinsic |
Alliance C-8H Strontium Ferrite Ceramic Magnetic Material |
|||
Magnetic Coercive Force, Hc | 3500 Oe | 3500 Oe | |
Alliance C-9B Strontium Ferrite Ceramic Magnetic Material |
|||
Magnetic Coercive Force, Hc | 3500 Oe | 3500 Oe | |
Alliance BIN-26 Bonded (Composite) Magnetic Material |