Magnetic Coercive Force, Hc 720 Oe
720 Oe
Alliance A-6 Alnico Magnetic Material
Magnetic Coercive Force, Hc 720 Oe
720 Oe
Intrinsic
Alliance A-6 Alnico Magnetic Material