Electrical Properties | Metric | English | Comments |
---|---|---|---|
Magnetic Remanence, Br | 10.1 Gauss | 10.1 Gauss | |
PSM Industries Pacific Sintered Metals Phosphorous Iron FP-1650-S Powdered Metal For applications requiring high yield strength and toughness. Magnetic properties superior to iron, but slightly inferior to silicon iron.Information Provided by Pacific Sintered Metals, a division .. |