Electrical Properties | Metric | English | Comments |
---|---|---|---|
Magnetic Remanence, Br | 7000 Gauss | 7000 Gauss | |
Pacific Sintered Materials FN-252-S Iron Nickel Soft Magnetic Powdered Metal Very low coercive force and high permeability. Excellent for shielding and switching applications.All information provided by Pacific Sintered Metals. |
|||
Magnetic Remanence, Br | 7000 Gauss | 7000 Gauss | |
Alliance A-2 Alnico Magnetic Material |