Electrical Properties | Metric | English | Comments |
---|---|---|---|
Magnetic Remanence, Br | 9700 Gauss | 9700 Gauss | |
Pacific Sintered Materials F-241-S1 Iron Soft Magnetic Powdered Metal Applications: DC magnetic applications such as pole pieces, cores, armatures, generator rotors and stator cores.Equivalent ASTM Specification: B310-70, TYPE III, CLASS AAll information provided by P.. |