Polymer Property : Curie Temperature = 200 °C Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Curie Temperature 200 °C
392 °F
PPT LSF120 Low Sintering Temperature Ferrite Powder
Uses: Low Temperature Co-fired Ceramic Components (LTCC), Multi-Layer Chip Inductors (MLCI), Chip Beads (EMI Suppressors)Electromagnetic proerties reported were tested on sintered toroids with a HP4..
Curie Temperature 200 °C
392 °F
Piezo Kinetics 552 Lead Zirconate Titanate Piezoelectric
Denoted as Navy Type VI, this ceramic is used as sensors that require extremely high dielectric constant and large displacements. PKI 556 material has been slightly modified to give a higher g33 val..
Curie Temperature 200 °C
392 °F
Tc
CeramTec Sonox® P51 Piezoceramic
Piezoceramic devices are used to convert mechanical features such as pressure or acceleration into voltages, or conversely, to convert a voltage into mechanical motion or oscillation. Piezoceramics ..