Electrical Properties Metric English Comments
Curie Temperature 340 °C
644 °F
Tc
CeramTec Sonox® P5 Piezoceramic
Piezoceramic devices are used to convert mechanical features such as pressure or acceleration into voltages, or conversely, to convert a voltage into mechanical motion or oscillation. Piezoceramics ..
Curie Temperature 340 °C
644 °F
Tc
CeramTec Sonox® P508 Piezoceramic
Piezoceramic devices are used to convert mechanical features such as pressure or acceleration into voltages, or conversely, to convert a voltage into mechanical motion or oscillation. Piezoceramics ..
Curie Temperature 340 °C
644 °F
Alliance N-35SH Neodymium Iron Boron Magnetic Material
Curie Temperature 340 °C
644 °F
Alliance N-38SH Neodymium Iron Boron Magnetic Material
Curie Temperature 340 °C
644 °F
Alliance N-40SH Neodymium Iron Boron Magnetic Material
Curie Temperature 340 °C
644 °F
Alliance N-42SH Neodymium Iron Boron Magnetic Material
Curie Temperature 340 °C
644 °F
Alliance N-33SH Neodymium Iron Boron Magnetic Material