Polymer Property : Curie Temperature = 350 °C Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Curie Temperature 350 °C
662 °F
PPT BP125 NiZn Ferrite Powder
Uses: EMI Suppressors, Wave Absorbing Tiles, Impeders, Multi-Hole Connectors, Inductors, Transformers, Converters, Choke Coils, AntennasElectromagnetic characteristics were tested on toroid with a H..
Curie Temperature 350 °C
662 °F
PPT FP350 Fully Sintered Ferrite Powder
Fully sintered NiZn ferrite, MnZn ferrite, and MgZn ferrite powders are available. Spherical or irregular particle shapes in custom particle sizes are available, ranging from sub-micron to a few hu..
Curie Temperature 350 °C
662 °F
Piezo Kinetics 402 Lead Zirconate Titanate Piezoelectric
Denoted as Navy Type I, it is designed to serve as a driver where high power and low losses are dictated by design. It is primarily well suited for ultrasonic cleaners and sonars.Elastic Compliance ..
Curie Temperature 350 °C
662 °F
Piezo Kinetics 502 Lead Zirconate Titanate Piezoelectric
Denoted as Navy Type II, it is designed for applications that require high electromechanical activity and high dielectric constant. These are used primarily as receivers e.g. hydrophones, phono pick..
Curie Temperature 350 °C
662 °F
Piezo Kinetics 700 Lead Zirconate Titanate Piezoelectric
This material has low dielectric constant, high QM, high shear coupling coefficient, good temperature stability and low aging characteristics. Common use of this material is in delay lines and accel..
Curie Temperature 350 °C
662 °F
Piezo Kinetics 802 Lead Zirconate Titanate Piezoelectric
Denoted as Navy Type III, it is specifically used as a driver that exhibits low losses under extreme driving conditions and has a high Q. PKI 804 is well suited for medical applications.Elastic Comp..
Curie Temperature 350 °C
662 °F
PPT LSF50 Low Sintering Temperature Ferrite Powder
Uses: Low Temperature Co-fired Ceramic Components (LTCC), Multi-Layer Chip Inductors (MLCI), Chip Beads (EMI Suppressors)Electromagnetic proerties reported were tested on sintered toroids with a HP4..
Curie Temperature 350 °C
662 °F
Tc
CeramTec Sonox® P504 Piezoceramic
Piezoceramic devices are used to convert mechanical features such as pressure or acceleration into voltages, or conversely, to convert a voltage into mechanical motion or oscillation. Piezoceramics ..
Curie Temperature 350 °C
662 °F
Goodfellow Cobalt/Silicon/Boron/Manganese Alloy
Information provided by Goodfellow.Composition Notes: Si + B content = 25 wt%. Fe+Mo content = 2 wt%.
Curie Temperature 350 °C
662 °F
Alliance N-28UH Neodymium Iron Boron Magnetic Material
Curie Temperature 350 °C
662 °F
Alliance N-30UH Neodymium Iron Boron Magnetic Material
Curie Temperature 350 °C
662 °F
Alliance N-35UH Neodymium Iron Boron Magnetic Material
Curie Temperature >= 350 °C
>= 662 °F
Channel Industries 5500 Lead Zirconate Titanate Piezoelectric
Navy Type IICharacterized by high coupling factors and high piezoelectric and dielectric constants over extended temperature ranges and stress amplitudes, lead zirconate titanates are the most exten..
Curie Temperature 350 °C
662 °F
Alliance N-33UH Neodymium Iron Boron Magnetic Material
Curie Temperature 350 °C
662 °F
PPT BP125HR NiZn Ferrite Powder
Uses: EMI Suppressors, Wave Absorbing Tiles, Impeders, Multi-Hole Connectors, Inductors, Transformers, Converters, Choke Coils, AntennasElectromagnetic characteristics were tested on toroid with a H..