Electrical Properties Metric English Comments
Curie Temperature 279 °C
534 °F
Carpenter Invar 36® Alloy, Annealed Bars and Strip
Data provided by Carpenter Technology Corporation.Carpenter Invar "36" alloy is a 36% nickel-iron alloy possessing a rate of thermal expansion approx. one-tenth that of carbon steel up to 200°C. T..
Curie Temperature 279 °C
534 °F
Carpenter Invar 36® Alloy, Cold Drawn Bars
Data provided by Carpenter Technology Corporation.Carpenter Invar "36" alloy is a 36% nickel-iron alloy possessing a rate of thermal expansion approx. one-tenth that of carbon steel up to 200°C. T..
Curie Temperature 279 °C
534 °F
Carpenter Invar 36® Alloy, Cold Rolled Strip
Data provided by Carpenter Technology Corporation.Carpenter Invar "36" alloy is a 36% nickel-iron alloy possessing a rate of thermal expansion approx. one-tenth that of carbon steel up to 200°C. T..