Electrical Properties Metric English Comments
Curie Temperature 380 °C
716 °F
Goodfellow Nickel Base Magnetic Shielding Alloy - Mu Metal
High Nickel magnetically soft alloy used for magnetic shielding, high quality but low noise audio frequency transformers, ground fault interrupter cores, anti-shoplifting devices, tape recorder head..