Polymer Property : Curie Temperature = 752 °F Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Curie Temperature 400 °C
752 °F
PPT BP80 NiZn Ferrite Powder
Uses: EMI Suppressors, Wave Absorbing Tiles, Impeders, Multi-Hole Connectors, Inductors, Transformers, Converters, Choke Coils, AntennasElectromagnetic characteristics were tested on toroid with a H..
Curie Temperature >= 400 °C
>= 752 °F
PPT LSF25 Low Sintering Temperature Ferrite Powder
Uses: Low Temperature Co-fired Ceramic Components (LTCC), Multi-Layer Chip Inductors (MLCI), Chip Beads (EMI Suppressors)Electromagnetic proerties reported were tested on sintered toroids with a HP4..
Curie Temperature 400 - 455 °C
752 - 851 °F
Special Metals INCOLOY® Alloy 907
A nickel-iron-cobalt alloy with additions of niobium and titanium for precipitation hardening. It has the low coefficient of expansion and high strength of INCOLOY alloy 903 but with improved notch..
Curie Temperature 400 - 455 °C
752 - 851 °F
Special Metals INCOLOY® Alloy 909
A nickel-iron-cobalt alloy with a silicon addition and containing niobium and titanium for precipitation hardening. It is similar to INCOLOY alloys 903 and 907 in that it has low thermal expansion ..
Curie Temperature 400 °C
752 °F
Special Metals NILOMAG® Alloy 77
A nickel-iron alloy with additions of copper and molybdenum. It is a low-loss, soft-magnetic alloy with a high initial permeability. Initial permeability 60,000; maximum permeability 300,000; satu..