Electrical Properties | Metric | English | Comments |
---|---|---|---|
Curie Temperature | 450 °C | 842 °F | |
Piezo Kinetics PKI 100 Lead Metaniobate Piezoelectric Lead Metaniobate exhibits properties not usually present in other types of piezoelectric ceramics. The noteworthy facts are its low mechanical QM, negligible aging, wide range of operating temperat.. |
|||
Curie Temperature | 450 - 500 °C | 842 - 932 °F | |
High Temp Metals Alloy 49 Iron-Nickel High Permeability Alloy, Bar, Cold Drawn High Permeability "49" alloy is a 48% nickel-iron alloy which has a saturation flux density of approximately 15,000 Gauss after hydrogen annealing. Hysteresis loss is very low in either DC or AC cir.. |
|||
Curie Temperature | 450 - 500 °C | 842 - 932 °F | |
High Temp Metals Alloy 49 Iron-Nickel High Permeability Alloy, Bar, Hydrogen Annealed at 2150°F (1177°C) High Permeability "49" alloy is a 48% nickel-iron alloy which has a saturation flux density of approximately 15,000 Gauss after hydrogen annealing. Hysteresis loss is very low in either DC or AC cir.. |
|||
Curie Temperature | 450 - 500 °C | 842 - 932 °F | |
High Temp Metals Alloy 49 Iron-Nickel High Permeability Alloy, Strip, Cold-Rolled High Permeability "49" alloy is a 48% nickel-iron alloy which has a saturation flux density of approximately 15,000 Gauss after hydrogen annealing. Hysteresis loss is very low in either DC or AC cir.. |
|||
Curie Temperature | 450 - 500 °C | 842 - 932 °F | |
High Temp Metals Alloy 49 Iron-Nickel High Permeability Alloy, Strip, Formed and Deep Draw Quality High Permeability "49" alloy is a 48% nickel-iron alloy which has a saturation flux density of approximately 15,000 Gauss after hydrogen annealing. Hysteresis loss is very low in either DC or AC cir.. |
|||
Curie Temperature | 450 - 500 °C | 842 - 932 °F | |
High Temp Metals Alloy 49 Iron-Nickel High Permeability Alloy, Bar, After Process Annealed at 1600°F (871°C) High Permeability "49" alloy is a 48% nickel-iron alloy which has a saturation flux density of approximately 15,000 Gauss after hydrogen annealing. Hysteresis loss is very low in either DC or AC cir.. |
|||
Curie Temperature | 450 - 500 °C | 842 - 932 °F | |
High Temp Metals Alloy 49 Iron-Nickel High Permeability Alloy, Bar, Cold Drawn High Permeability "49" alloy is a 48% nickel-iron alloy which has a saturation flux density of approximately 15,000 Gauss after hydrogen annealing. Hysteresis loss is very low in either DC or AC cir.. |
|||
Curie Temperature | 450 - 500 °C | 842 - 932 °F | |
High Temp Metals Alloy 49 Iron-Nickel High Permeability Alloy, Bar, Hydrogen Annealed at 2150°F (1177°C) High Permeability "49" alloy is a 48% nickel-iron alloy which has a saturation flux density of approximately 15,000 Gauss after hydrogen annealing. Hysteresis loss is very low in either DC or AC cir.. |
|||
Curie Temperature | 450 - 500 °C | 842 - 932 °F | |
High Temp Metals Alloy 49 Iron-Nickel High Permeability Alloy, Strip, Cold-Rolled High Permeability "49" alloy is a 48% nickel-iron alloy which has a saturation flux density of approximately 15,000 Gauss after hydrogen annealing. Hysteresis loss is very low in either DC or AC cir.. |
|||
Curie Temperature | 450 - 500 °C | 842 - 932 °F | |
High Temp Metals Alloy 49 Iron-Nickel High Permeability Alloy, Strip, Formed and Deep Draw Quality High Permeability "49" alloy is a 48% nickel-iron alloy which has a saturation flux density of approximately 15,000 Gauss after hydrogen annealing. Hysteresis loss is very low in either DC or AC cir.. |
|||
Curie Temperature | 450 °C | 842 °F | |
Goodfellow Nickel/Iron/Molybdenum Alloy Information provided by Goodfellow. |
|||
Curie Temperature | 450 °C | 842 °F | |
Alliance BIF-11 Bonded (Composite) Magnetic Material |
|||
Curie Temperature | 450 °C | 842 °F | |
Alliance BIF-17 Bonded (Composite) Magnetic Material |
|||
Curie Temperature | 450 °C | 842 °F | |
Alliance BIF-19 Bonded (Composite) Magnetic Material |
|||
Curie Temperature | 450 °C | 842 °F | |
Alliance BIF-2 Bonded (Composite) Magnetic Material |
|||
Curie Temperature | 450 °C | 842 °F | |
Alliance C-5 Strontium Ferrite Ceramic Magnetic Material |
|||
Curie Temperature | 450 °C | 842 °F | |
Alliance C-7 Strontium Ferrite Ceramic Magnetic Material |
|||
Curie Temperature | 450 °C | 842 °F | |
Alliance C-7B Strontium Ferrite Ceramic Magnetic Material |
|||
Curie Temperature | 450 °C | 842 °F | |
Alliance C-8 Strontium Ferrite Ceramic Magnetic Material |
|||
Curie Temperature | 450 °C | 842 °F | |
Alliance C-8H Strontium Ferrite Ceramic Magnetic Material |
|||
Curie Temperature | 450 °C | 842 °F | |
Alliance C-9 Strontium Ferrite Ceramic Magnetic Material |
|||
Curie Temperature | 450 °C | 842 °F | |
Alliance C-9B Strontium Ferrite Ceramic Magnetic Material |
|||
Curie Temperature | 450 °C | 842 °F | |
Alliance BIF-16 Bonded (Composite) Magnetic Material |
|||
Curie Temperature | 450 °C | 842 °F | |
Alliance C-8B Strontium Ferrite Ceramic Magnetic Material |
|||
Curie Temperature | 450 °C | 842 °F | |
PPT BP40 NiZn Ferrite Powder Uses: EMI Suppressors, Wave Absorbing Tiles, Impeders, Multi-Hole Connectors, Inductors, Transformers, Converters, Choke Coils, AntennasElectromagnetic characteristics were tested on toroid with a H.. |
|||
Curie Temperature | 450 - 500 °C | 842 - 932 °F | |
High Temp Metals Alloy 49 Iron-Nickel High Permeability Alloy, Bar, After Process Annealed at 1600°F (871°C) High Permeability "49" alloy is a 48% nickel-iron alloy which has a saturation flux density of approximately 15,000 Gauss after hydrogen annealing. Hysteresis loss is very low in either DC or AC cir.. |