Electrical Properties Metric English Comments
Curie Temperature 95.0 °C
203 °F
PPT FP95 Fully Sintered Ferrite Powder
Fully sintered NiZn ferrite, MnZn ferrite, and MgZn ferrite powders are available. Spherical or irregular particle shapes in custom particle sizes are available, ranging from sub-micron to a few hu..
Curie Temperature 95.0 °C
203 °F
PPT BP2000 NiZn Ferrite Powder
Uses: EMI Suppressors, Wave Absorbing Tiles, Impeders, Multi-Hole Connectors, Inductors, Transformers, Converters, Choke Coils, AntennasElectromagnetic characteristics were tested on toroid with a H..
Curie Temperature <= 95.0 °C
<= 203 °F
Special Metals DURANICKEL® 301 (UNS N03301) Annealed and Aged Rod and Bar
Tensile strength (ultimate and yield), compressive strength, hardness, and elongation values reported here are typical for Annealed and Aged Rod and Bar specifically. Other property values are typic..
Curie Temperature <= 95.0 °C
<= 203 °F
Special Metals DURANICKEL® 301 (UNS N03301) Annealed and Aged Strip
Tensile strength (ultimate), hardness, and elongation values reported here are typical for Annealed and Aged Strip specifically. Other property values are typical of aged DURANICKEL® alloy 301 or..
Curie Temperature <= 95.0 °C
<= 203 °F
Special Metals DURANICKEL® 301 (UNS N03301) Annealed and Aged Wire
Tensile strength (ultimate) and elongation values reported here are typical for Annealed and Aged Wire specifically. Other property values are typical of aged DURANICKEL® alloy 301 or the alloy i..
Curie Temperature <= 95.0 °C
<= 203 °F
Special Metals DURANICKEL® 301 (UNS N03301) Cold-Drawn and Aged Rod and Bar
Tensile strength (ultimate and yield), compressive strength, hardness, and elongation values reported here are typical for Cold-Drawn and Aged Rod and Bar specifically. Other property values are typ..
Curie Temperature <= 95.0 °C
<= 203 °F
Special Metals DURANICKEL® 301 (UNS N03301) Half-Hard and Aged Strip
Tensile strength (ultimate), hardness, and elongation values reported here are typical for Half-Hard and Aged Strip specifically. Other property values are typical of aged DURANICKEL® alloy 301 o..
Curie Temperature <= 95.0 °C
<= 203 °F
Special Metals DURANICKEL® 301 (UNS N03301) Hot-Finished and Aged Rod and Bar
Tensile strength (ultimate and yield), hardness, and elongation values reported here are typical for Hot-Finished and Aged Rod and Bar specifically. Other property values are typical of aged DURANIC..
Curie Temperature <= 95.0 °C
<= 203 °F
Special Metals DURANICKEL® 301 (UNS N03301) Spring Strip, Aged
Tensile strength (ultimate), hardness, and elongation values reported here are typical for Spring Strip, Aged specifically. Other property values are typical of aged DURANICKEL® alloy 301 or the ..
Curie Temperature <= 95.0 °C
<= 203 °F
Special Metals DURANICKEL® 301 (UNS N03301) Spring Wire, Aged
Tensile strength (ultimate) and elongation values reported here are typical for Spring Wire, Aged specifically. Other property values are typical of aged DURANICKEL® alloy 301 or the alloy in gen..
Curie Temperature 95.0 - 105 °C
203 - 221 °F
Goodfellow Ni-Mn-Ga Magnetic Shape Memory Alloy (MSM)
Ni50Mn28.5Ga21.5 single crystal. The magnetic shape memory phenomenon is produced by magnetic-field-induced rearrangement of (ferromagnetic) twinned martensite microstructure accompanied by a large ..