High Voltage Arc-Tracking Rate, HVTR 4.00 - 18.0 mm/min
0.157 - 0.709 in/min
Average value: 13.2 mm/min Grade Count:6
Overview of materials for Polyphthalamide (PPA), 50% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 50% Glass Fiber Reinforced". Each property range of values reported is minimum and maxi..
High Voltage Arc-Tracking Rate, HVTR 4.00 mm/min
0.157 in/min
Solvay Specialty Polymers Amodel® AF-1550 V0 Polyphthalamide (PPA) Resin, 50% Glass/Mineral Reinforced, Dry As Molded &
Data provided by the manufacturer, Amoco Corporation.AMODEL AF-1550 V0 resin is a 50% glass/mineral reinforced, flame retarded polyphthalamide (PPA) that features: high deflection temperature, high ..