Electrical Properties Metric English Comments
Dielectric Strength 0.0209 kV/mm
0.530 kV/in
Zircar Refractory Composites RS-DR Refractory Sheet
TYPE RS-DR is a rigid pre-fired sheet that has been heat-treated to remove all organic binder and is stable to moisture attack. Refractory Sheet Type RS-DR is suited for use as a setter or barrier f..