Polymer Property : Dielectric Strength = 0.315 kV/mm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 0.315 kV/mm

@Thickness 3.17 mm
8.00 kV/in

@Thickness 0.125 in
Unconditioned; ASTM D149
Garlock 9200 Nitrile Rubber Gasketing, Nylon Insert
Nitrile rubber with proprietary nylon insertCombines elasticity and extensibility of rubber with strength of fabric insert. Specially compounded in varying burst strengths for almost any service co..