Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 1.50 kV/mm | 38.1 kV/in | ASTM D149-95a |
Thermoseal KLINGERSIL® C-4500 Carbon Fiber Reinforced Gasketing Carbon FiberNitrile BinderHigh TemperatureHigh Internal PressureSuitable for a Wide Range of Chemical ApplicationsGood Steam SheetInformation provided by Thermoseal Inc. |
|||
Dielectric Strength | 1.50 kV/mm | 38.0 kV/in | 0.1" gap |
3M Fluorinert™ FC-72 Electronic Liquid 3M™ Fluorinert™ Liquid FC-72 is a non-conductive, thermally and chemically stable liquid ideal for many direct contact single and two phase low temperature heat transfer applications, in testing, .. |